Mugihe cyibigeragezo, inenge zifata akenshi zibaho nta guhanura byanze bikunze, bityo injeniyeri nziza yikigereranyo igomba kuba ifite uburambe bukomeye bwo gusuzuma impamvu byihuse, kuko ibiciro byiyongera mugihe cyakoreshejwe mumashini itera inshinge.
Hano itsinda ryacu ryakusanyije ubunararibonye, niba uku kugabana gushobora kwerekana akantu gato kugirango twungukire gukemura ibibazo bisa, tuzishima cyane.
Hano turavuga ku bimenyetso bitatu: “Ibimenyetso byatwitse”, “Ibimenyetso bitose” na “Ikimenyetso cy'ikirere”.
Ibiranga:
·Kugaragara Rimwe na rimwe
·Kugaragara mugice gito cyambukiranya cyangwa umwanya wumutego wikirere
·Ubushyuhe bwo gushonga ni hafi yo hejuru yubushyuhe bwo gutera
·Inenge igira ingaruka runaka mukugabanya umuvuduko wibikoresho
·Igihe cya plastike ni kirekire cyane, cyangwa guma mumwanya wimbere wikinyamakuru kinini
·Ibikoresho bya pulasitiki byongeye gukoreshwa bikoreshwa cyane cyangwa ibikoresho byashongeshejwe inshuro nyinshi mbere
·Kugaragara mububiko hamwe na sisitemu yo kwiruka
·Ibumba ifunze nozzle (Hagarika Nozzle)
Ibiranga:
3 Mark Ikimenyetso cy'ikirere
Muri rusange, imiterere yikimenyetso cyikirere kirakomeye, gifite ifeza cyangwa ibara ryera, bikunze kugaragara hejuru yubuso / bugoramye, imbavu / uburebure bwurukuta bihindura ahantu cyangwa hafi ya nozzle, ubwinjiriro bw irembo bugaragara nkurwego ruto rwerekana ikirere; Ibimenyetso byikirere nabyo bigaragara mugushushanya, kurugero: gushushanya inyandiko cyangwa kwiheba ahantu.
Usibye ubwoko bwavuzwe haruguru, dufite kandi "Ikirahure-fibre" na "Ibara ryamabara" kuruhande rwibice.none mugihe kizaza, inenge nyinshi zifatika zizasangirwa ninshuti nkoramutima kuri linkedin, niba ufite ibitekerezo bitandukanye kubyerekeye inyandiko yanjye, nyamuneka ineza umenyeshe ibitekerezo byawe, nkuko tubizi, linkedin burigihe ni urubuga rwiza kuri twe gusangira, kwiga no kunoza!